BÖHLER N352S1 is a martensitic chromium steel with nickel addition. Heat treatable grade, capable of taking a mirror finish. Higher corrosion resistance compared to 13% chromium steel. Resistant to the effects of seawater, weak acids and alkaline solutions, as well as to acids having a strong, oxidizing effect such as nitric acid. Surface finish for optimum corrosion resistance: fine ground or polished.
For components subject to high mechanical and corrosive stress, e.g. screws and shafts, at operating temperatures up to approx. 752° F.

Available Product Shapes

Long Products: ) Presented data refer exclusively to long products. Please observe the detailed explanations at the end of the data sheet (pdf).

Melting Route

Airmelted

Material Numbers

Market grade
431
EN
X15CrNi17-3

Standards

BS
S80

Chemical Composition

* Chemical Composition (Average %)

C
0.12 to 0.20
Si
max. 1.0
Mn
max. 1.0
P
max. 0.030
S
max. 0.025
Cr
15 to 18.0
Mo
max. 0.30
Ni
2.0 to 3.0
V
max. 0.20
W
max. 0.05
Cu
max. 0.30
Co
max. 0.05
Ti
max. 0.05
Nb
max. 0.05
Fe
REM